Dynamic contact behavior of graphite-like carbon films on ductile substrate under micro-scale impact

In our recent collaborative study published in Surface and Coatings Technology, micro-impact testing revealed marked coating thickness dependent changes in the fracture behavior of graphite-like carbon films on a soft stainless steel substrate subjected to multiple impacts.