Insights into Indentation Cracking at Elevated Temperatures: another ground-breaking publication with the NanoTest Xtreme Understanding the interplay between fracture and plasticity at small scale is absolutely critical to the reliability of new materials and technologies. Researchers at the University of Oxford and thei... 23 Jul 2026 Company News
New paper in Tribology International: Length scale effects on the fretting wear of DLC coating system The latest collaboration between Micro Materials' Prof Ben Beake and Dr Stephen Goodes, Prof Tomasz Liskiewicz at Manchester Metropolitan University and Dr Sam McMaster at ARU has just been published ... 18 May 2026 Company News
Synergistic Fretting -Corrosion Mechanisms in DLC Coatings In his invited talk at ICMCTF 2026, Prof Tomasz Liskiewicz, Manchester Metropolitan University, reported on collaborative work developing multilayer DLC coating systems to protect implants. He describ... 5 May 2026 Company News
Micro Impact testing to develop multilayer coating systems with Enhanced Durability - Micro Materials presents at ICMCTF on joint stand with Rtec Instruments For the first time, Micro Materials exhibited alongside Rtec Instruments on stand 308 at ICMCTF 2026 in San Diego. Krish Narain and Vishal Khosla welcomed visitors to discuss theexciting prospects ope... 23 Apr 2026 Events
Rtec Instruments Inc acquires Micro Materials Ltd Rtec Instruments, a global leader in surface characterization and tribology solutions, today announced the acquisition of Micro Materials Ltd., a UK-based pioneer in advanced micro- and nanoindentatio... 23 Mar 2026 Company News
Sales success in cutting tools sector for Micro Materials Ltd We are delighted to announce that Micro Materials Ltd has recently delivered a NanoTest Vantage system to YG-1 Co Ltd's HQ, located in Incheon, South Korea's third largest city. Established in 1981, Y... 13 Mar 2026 Company News
The spatially-distributed impact test - a new video with case studies now available on Micro Materials Ltd's You Tube channel Did you know that the spatially-distributed impact test—an extension of conventional nano- and micro-impact testing—was pioneered by the applications specialists at Micro Materials Ltd using the NanoT... 6 Feb 2026 Company News
Visit to Liaoning Academy of Materials in Shenyang During a recent customer care visit to Liaoning Academy of Materials in Shenyang,Dr Krish Narain , Micro Materials Ltd ’s Director of Business Development, enjoyed the privilege of meeting Professor Y... 27 Jan 2026 Company News
New Paper - TiN, CrN and TiCrN coating architectures on M2 steel: consequences for wear and micro-impact resistance Micro Materials is pleased to announce the publication of a new study evaluating the mechanical, tribological, and impact performance of three arc-evaporated multilayer coatings deposited on hardened ... 19 Jan 2026 Company News
Micro Materials presents at Reactive Sputter Deposition and thin films symposium (RSD2025) organised by Manchester Metropolitan University Recent achievements in reactive sputter deposition and thin films were under the spotlight at this week'sinternational symposium in Manchesteron Reactive Sputter Deposition. Organised by Professor Pet... 18 Dec 2025 Events
New Paper - High temperature indentation La-Fe-Co-Si alloys are promising magnetocaloric materials for future cooling applications. Researchers at the Korea Institute of Materials Science have been using the precision indent placement and ex... 18 Nov 2025 Company News
9th Dec 2025 -Online symposium - The state of the art in impact testing: how to improve your materials' performance The state of the art in impact testing: how to improve your materials' performance the title of this year'sMicro Materials Ltd's online mini symposium. Registration is open now. With our NanoTest Vant... 10 Nov 2025 Events