The latest in the MML Application Note
series describes the unrivalled capability of the High Temperature
Testing option for the NanoTest.
Included in the note are:
1) A discussion on why
the use of a heated indenter is essential.
2) A discussion of
Nanoscale Glass transition behaviour
3) A section on impact
measurements at high temperatures.
4) Further Applications
of high temperature testing: Phase Changes for
Shape Memory Alloys
Adhesion - Variation of pull-off forces with
temperature.
To request a copy of this application note,
please contact us
|